Sachiya Steel International is one of the well-known Manufacture and Exporter for Hastelloy C22 Wire Mesh , which can be welded by all common methods and are highly versatile. Displaying excellent resistance to stress corrosion cracking and non – oxidizing acids, Hastelloy C22 Hexagonal Wire Mesh have been used for numerous applications. Hastelloy C22 Welding Wire Mesh is the most versatile of the Alloys and is widely used for chemical process equipment applications due to their excellent resistance to non – oxidizing environments.
Water – base coolant should be premium quality for Hastelloy C22 Netting Wire Mesh, sulfochlorinated water soluble oil or chemical emulsion with extreme pressure additives. Water – base coolant of Hastelloy C22 Woven Wire Mesh may cause chipping and rapid failure of carbide tools in interrupted cuts. Hastelloy C22 Spring Steel Wire Mesh is an alloy that is precipitation harden able for high mechanical properties.
Alloy C22 Hexagonal Wire Mesh maintains good strength and oxidation resistance at temperatures up to about 1300 Degree F (700 Degree C). The high strength and excellent fabrication characteristics of Alloy C22 Welding Wire Mesh make it useful for various components of aircraft and industrial gas turbines. Alloy C22 Netting Wire Mesh has good resistance to corrosion and oxidation along with high tensile and creep-rupture properties at temperatures to 1300 Degree C. Applications of Alloy C22 Woven Wire Mesh include blades, vanes, shafts, tail cones, afterburners, springs, and fasteners.
|
Hastelloy C22 Wire mesh Specifications
|
||
| Specifications | : | ASTM / ASME B574 / SB574 |
| Standard | : | ASTM, ASME |
| Size | : | 15NB to 150NB In |
| Types | : | Wire Mesh, Hexagonal Wire mesh, Welding Wire mesh, Netting Wire mesh, Woven Wire mesh, Spring Steel wire mesh, Fencing Wire mesh etc. |
| Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
| C22 | 0.010 max | 0.50 max | 0.08 max | 0.02 max | 2.50 max | 50.015 min* | 20.00 – 22.50 | 2.00 – 6.00 | 12.50 – 14.50 | 0.02 max |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Hastelloy C22 | 8.69 g/cm3 | 1399 °C (2550 °F) | Psi – 1,00,000 , MPa – 690 | Psi – 45000 , MPa – 310 | 45 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | GOST | EN | OR |
| Hastelloy C22 | 2.4602 | N06022 | NW 6022 | – | NiCr21Mo14W | – |
- Off-Shore Oil Drilling Companies
- Power Generation
- Petrochemicals
- Gas Processing
- Specialty Chemicals
- Pharmaceuticals
- Pharmaceutical Equipment
- Chemical Equipment
- Sea Water Equipment
- Heat Exchangers
- Condensers
- Pulp and Paper Industry